A270 TP316L Seamless Stainless Steel Tube
GNEE manufactures and supplies A270 TP316L stainless steel pipe. With many years of experience, GNEE produces high-diameter pipes suitable for many industries.
A270 TP316L austenitic stainless steel pipe contains a high molybdenum content in its chemical composition, which can improve its corrosion resistance, especially for equipment in some highly corrosive environments.
In addition, compared with 310 and 304 stainless steel, A270 TP316L seamless pipe shows better performance under high temperature conditions, especially in environments with sulfuric acid concentrations below 15% or above 85%.
Therefore, A270 TP316L stainless steel pipe is widely used in industrial and food processing fields with high requirements for hygiene standards, such as baking, beverages, cosmetics, dairy products, food or pharmaceutical industries.
ASTM A270 Tp316l Seamless Polished inside Tube Mechanical Properties
| º F(º C) | |||||
| TP316L | 1900(1040) | 25(170) | 70(485) | 35 |
A270 Tp316l Seamless
| Specific Heat 0-100 degree (J/kg.K) | Density (kg/m3) | ||||||||
| at 100 degree | at 500 degree | 0-100 degree | 0-315 degree | 0-538 degree | |||||
| TP316L | 500 | 8000 | 193 | 16.2 | 21.5 | 17.2 | 17.8 | 18.4 | 720 |
A270 TP316L Seamless steel pipe

Gnee company covers an area of 35,000 square meters and has more than 200 employees, including 80 technical staff. We have established an effective and complete quality control and assurance system. The company has also obtained ISO9001 quality system certification.

1.Q.Why choose you?
A.Firstly quality, secondly price, we can give you both. Our service formula: good quality + good price + good service=customer's trust.
2.Q.Can your products be customized?
3.Q.Do you have quality control?
ป้ายกำกับยอดนิยม: a270 tp316l seamless stainless steel tube, China a270 tp316l seamless stainless steel tube manufacturers, suppliers, factory, ท่อสแตนเลสสำหรับกิจกรรมทางวัฒนธรรม, ท่อสแตนเลสสำหรับการฉายภาพยนตร์, ท่อสแตนเลสสำหรับการสำเร็จการศึกษา, ท่อสแตนเลสสำหรับการผลิตละคร, ท่อสแตนเลสสำหรับงานแต่งงาน, ท่อสแตนเลสสำหรับการประชุมเชิงปฏิบัติการ
คุณอาจชอบ
ส่งคำถาม